True skin-type waterproofing, construction efficiency far exceeds old-age materials
The coating is composed of two components, A and B. Component A is the main agent, which is a mixture of anionic synthetic rubber, microemulsion made by special process and various chemical additives. The rubber component is a continuous phase, which can greatly enhance the elongation and puncture resistance of the material after film formation, while the B component is a coagulant, which is an aqueous solution prepared by metal salts and other electrolytes with corresponding concentration. However, in order to ensure the molecular stability of this component, it is usually kept in powder form
1. true skin-type waterproofing, the product cured to form a seamless, continuous waterproof membrane, no lap leakage potential.
2. products with elongation (more than 1200%) and recovery rate (90%).
Construction efficiency far exceeding that of old era materials, fast construction speed.
Curing within 3 seconds after the coating is sprayed, and no hanging on the vertical wall construction.
Can be constructed on moist substrates with water content ≤ 80%.
Real safe coating, spraying cold construction, no need to heat, safe construction.
No volatile solvents, green and environmentally friendly.
—Underground structure outside waterproofing: subway, building basement, common trench (cable, optical cable trench), etc.; roof waterproofing: concrete flat roof, color steel sandwich insulation board, slate tile, bunker trench, etc.; artificial water lake, pool, waste disposal site, sink, golf course water pond, etc.; underground channel, waste water treatment plant, swimming pool inside and outside waterproofing and anti-corrosion; bridge waterproofing; vehicle chassis and ship's anti-corrosion, anti-fouling.
Substrate acceptance-cleaning substrate-detail protection
Additional layer of detail construction - Large area spraying - Quality inspection and acceptance
Quality acceptance (water drenching, water storage test)-protective layer construction
Cannot be used in rainy weather or with rain within 12 hours.
The substrate should be solid and flat, no oil, sand, shelling; can be wet, but there should be no open water, while the drainage slope of the grass-roots level should meet the design requirements; penetrate the waterproofing layer of the pipeline, pre-buried parts, equipment foundations, reserved holes, etc. should be buried and installed firmly before the construction of the waterproofing layer;.
The base layer yin and Yang corners and the root of the pipe should be plastered into arc and strengthen the additional layer, the radius of the arc is 50mm, the width of the additional layer is 300mm per side; the gun should be tested before the large area construction spraying, and the spraying operation should be crossed horizontally and vertically.
After the completion of the waterproof layer for quality acceptance, acceptance after the construction of the protective layer, can not be used in more than 5 levels of windy weather conditions.